What thickness of boards can I measure?

Depending on the model of meter, you can accurately measure boards as thin as 1/2″ and up to 1-1/2″ thick.

Note: Make sure there is nothing behind boards less than 1″ thick when you take the measurement because Wagner Meters handheld moisture meters will read through the thinner board and measure the moisture in the material behind. Under no circumstances should you measure a piece of wood that is sitting on a metal table.