What depth do I measure at when new concrete has been poured on an old slab?

Please Note: This is somewhat out of the norm and is not covered by the ASTM F2170 standard. The following answer is based on information we have received from experts.

Example:

An existing five-year-old, four-inch slab has three inches of new cement added to it. The total thickness is seven inches.

Excessive moisture from any area in the combined slab can cause a failure. It is best to test the moisture in the center of the old slab as well as the center of the freshly poured slab.