How many relative humidity tests should I use on each job?

As part of the project documentation process, ASTM F2170 requires that 3 tests be placed in the first 1,000 square feet and that one test is placed every 1,000 square feet thereafter. If you are using the Rapid RH® system as a monitoring tool early in a project to determine when final acceptance testing should be performed, several Smart Sensors can be placed throughout the floor as soon as 28 days after the pour and readings taken as often as desired.